DESCRIPTION
|
UNIT
|
WARP
|
WEFT
|
|
Polyester filament Yarn
|
Denier
|
FY75
|
FY100
|
|
Conductive Yarn
|
Denier
|
97D
|
97D
|
|
Weaving Structure
|
Twill
|
2UP 1DOWN
|
|
|
Pattern
|
Grid
|
5mm
|
5mm
|
|
Weight
|
GR/YD
|
150
|
|
|
Density
|
Inch
|
186
|
94
|
|
Tensile Strength
|
KG
|
102
|
65
|
|
Width
|
Inch
|
58/60
|
|
|
Conductive Yarn
|
BASF
|
||
|
Surface Resistivity
|
§Ù/§¯
|
5E
|
|
|
Frictional Electronic Voltage Volt |
Cotton
|
less than 100V
|
|
|
Nylon
|
less than100v
|
||
|
Half Decay Time
|
Sec
|
0.3
|
|
|
Particle Cleaniness
|
0.3§/§¤
|
4
|
|
|
0.5§/§¤
|
2
|
||
|
Particle Filtration Efficiency
|
0.3§/§¤
|
92
|
|
|
0.5§/§¤
|
94
|
||
|
Moisture Permeability
|
G/§³/24hr
|
10,800
|
|
|
Air Permeability
|
§¨/§²sec
|
3.6
|
|
|
Class
|
10~100
|
||


This
ESD and MICRO Contamination control
fabric is sutiable for
Microelectronics
Semiconductor
Biotechnical
Pharmaceutical
Food
processing
industries
|
Color Reference
|
|||||||
|
White
|
Blue
|
Sky Blue
|
Navy Blue
|
Green
|
Light Green
|
Olive Green
|
Pink
|
Special attention to use Polyester ESD fabric.
Polyester is dissolved by Alkali just same as regular polyester, so customer should avoid the following treatment.
Polyester can be damaged by alkali especailly on conductive layer, because conductive carbon will be dissoved out by alkali treatment. The same problem will happen by color repair treatment byalkali in the dyed fabric.